DSC test: Determine the thermal properties of your materials

What is a DSC?

DSC (Differential Scanning Calorimetry) is an analytical technique used to measure thermal properties of materials.
The instrument measures the heat flow to a sample compared to a reference, while the temperature is changed in a controlled manner.

At Deon Research Centre, we use DSC to analyse polymers, resins, composites and additives to understand:

  • Glass transition temperature (Tg)
  • Melting points and crystallization behavior
  • Curing kinetics of thermosets
  • Specific heat capacity and stability

This data is essential for material development, quality control and process optimization.

Witte en lichtgrijze zeshoekige patronen met een vervaagde overgang naar een witte achtergrond.

Why choose a DSC at Deon Research Centre?

Our DSC measurements combine precision, repeatability and material expertise:

  • Accurate thermal characterization
    Detect subtle thermal transitions and exothermic/endothermic reactions.
  • Supporting material development
    Optimise formulations of resins, polymers and composites based on thermal properties.
  • Process optimization and quality control
    Check consistency between batches, monitor curing rates and predict material properties.
  • Wide range of applications
    Suitable for polymers, resins, composites, additives and coatings in R&D and production.

How does DSC work?

The use of DSC includes the following phases:

  1. Sample preparation: The material sample is prepared and placed in a special pan for analysis. Deon Research Centre ensures correct sample preparation in accordance with relevant standards.
  2. Differential calorimetry: The sample and a reference are heated or cooled evenly. The DSC device measures the difference in heat flux between them to document thermal transitions. Our equipment is calibrated for optimal accuracy.
  3. Data analysis: The collected data is analyzed to identify the possibilities of thermal transitions and to determine material properties, such as melting temperature, glass transition, or crystallization. Deon Research Centre provides detailed reports with clear analyses.

DSC applications in industry

Deon Research Centre is involved in the application of DSC in various sectors:

  • Polymer industry: determination of melting temperature and crystallinity of polymers for processing and manufacturing. DSC helps to optimize production processes.
  • Pharmaceutical industry: drug analysis for thermal stability and homogeneous mixability. Deon Research Centre complies with the most stringent quality standards for pharmaceutical tests.
  • Food industry: assessment of fat and oil stability under different thermal conditions. Deon Research Centre supports the food industry with comprehensive material analyses.

What does this mean for your company?

A DSC analysis at Deon Research Centre provides accurate and reproducible thermal characterization of polymers, resins, composites and additives. Our advanced equipment and expert analysts provide reliable data, essential for material development, quality control and process optimization.

FAQ

DSC test: Determine the thermal properties of your materials

What types of materials can be analysed with DSC?

DSC can be applied to a wide range of materials, including polymers, pharmaceuticals, food components, and metals. Contact us for specific questions about your materials.

How long does a typical DSC analysis take?

Duration varies based on the specific material and analysis methods; please contact us for more detailed time estimates.

Can DSC analyses help identify glass transition temperatures?

Yes, DSC is highly effective in measuring and identifying glass transition temperatures and other thermal transitions.

Does Deon Research Centre follow recognized standards when performing DSC analyses?

Yes, our DSC analyses are performed according to internationally recognized standards, such as ISO 11357 and ASTM E1356, to ensure the highest quality standards.

Contact person Deon

Get in touch with us!

Are you interested in how DSC can improve your materials research and development? Contact Deon Research Centre today for more information and find out how we can support your business with high-quality thermal analysis!